A solution to the flaking of the sealing strip by spraying(spraying) paint after sealing
1. The sealing edge does not reach the highest bond strength, check whether the operation is reasonable, or whether the type of hot melt glue is selected correctly;
2. Cover the paint off the wood skin, check whether the back of the wood skin is too much grease or the back of non-woven cloth(paper) and whether the wettability of the plate is up to the standard;
3. Seal the paint off the wood skin, check whether the wood skin is too thin holes, whether the solvent of the paint penetrates into the glue to destroy the film;
4. When sealing the edge, the treatment is not good, the rubber line is too thick, resulting in poor closure, and the solvent easily penetrates into the adhesive film damage strength.